IB - 900
No | Specification | IB - 900 |
1 |
Max. Service Temperature (Temperature Kerja Maximum) (0C) |
900 |
2 |
Bulk Density (Berat Jenis) (gr/cm3) |
0.46 |
3 |
Cold Crushing Strenght (Kuat Tekan) (kg/cm2) |
> 5 |
4 |
Thermal Conductivity at 350 0C (kcal/mh0C) |
0.13 |
5 |
Chemical Composition (Komposisi Kimia) AI2O3 (%) SiO2 (%) |
> 20 > 65 |
B - 1
No | Specification | B -1 |
1 |
Max. Service Temperature (Temperature Kerja Maximum) (0C) |
950 |
2 |
Bulk Density (Berat Jenis) (gr/cm3) |
0.70 |
3 |
Cold Crushing Strenght (Kuat Tekan) (kg/cm2) |
> 25 |
4 |
Thermal Conductivity at 350 0C (kcal/mh0C) |
0.17 |
5 |
Chemical Composition (Komposisi Kimia) AI2O3 (%) SiO2 (%) |
> 25 < 65 |
B - 2
No | Specification | B - 2 |
1 |
Max. Service Temperature (Temperature Kerja Maximum) (0C) |
1000 |
2 |
Bulk Density (Berat Jenis) (gr/cm3) |
0.75 |
3 |
Cold Crushing Strenght (Kuat Tekan) (kg/cm2) |
> 25 |
4 |
Thermal Conductivity at 350 0C (kcal/mh0C) |
0.18 |
5 |
Chemical Composition (Komposisi Kimia) AI2O3 (%) SiO2 (%) |
> 30 < 60 |
C - 1
No | Specification | C - 1 |
1 |
Max. Service Temperature (Temperature Kerja Maximum) (0C) |
1200 |
2 |
Bulk Density (Berat Jenis) (gr/cm3) |
1.05 |
3 |
Cold Crushing Strenght (Kuat Tekan) (kg/cm2) |
> 50 |
4 |
Thermal Conductivity at 350 0C (kcal/mh0C) |
0.30 |
5 |
Chemical Composition (Komposisi Kimia) AI2O3 (%) SiO2 (%) |
> 35 < 60 |
C - 2
No | Specification | C - 2 |
1 |
Max. Service Temperature (Temperature Kerja Maximum) (0C) |
1350 |
2 |
Bulk Density (Berat Jenis) (gr/cm3) |
1.10 |
3 |
Cold Crushing Strenght (Kuat Tekan) (kg/cm2) |
> 60 |
4 |
Thermal Conductivity at 350 0C (kcal/mh0C) |
0.35 |
5 |
Chemical Composition (Komposisi Kimia) AI2O3 (%) SiO2 (%) |
> 45 < 55 |